Good 3D PETG settings start with a hotter nozzle than PLA, a warm bed, gentle part cooling and short retraction. Get those four right and PETG gives glossy, tough parts that flex before they snap, which is why it suits outdoor brackets and mechanical pieces.
Quick Answer
Print PETG at about 230 to 250 degrees on the nozzle and 70 to 85 on the bed, with the fan at 30 to 50 percent after the first layers. Keep retraction short and speeds moderate. Dry the spool first, as damp PETG strings badly. A spool to tune on usually costs R249 to R399.
🌡️ Nozzle and bed temperature
The spool label sets the range, and most land between 230 and 250 degrees. Start in the middle and print a small test cube. If it strings and looks cloudy, drop 5 degrees. If layers peel apart, raise it.
Bed temperature is 70 to 85 degrees. Print the first layer slightly further from the bed than you would with PLA, because PETG sticks very firmly and a squashed first layer can bond to a smooth PEI sheet.
Run the first layer a few degrees hotter than the rest if corners lift, and slow it to roughly 20 mm/s so the plastic wets the surface. After that, 40 to 60 mm/s is a comfortable range for walls on a standard 0.4 mm nozzle. Fast printing needs more heat to keep layers fused, so if you raise speed, raise temperature by 5 degrees before judging the result.
Keep a notebook of what worked for each brand and colour, because two PETG spools from different makers rarely behave identically, and transparent or glittery colours often want a slightly different temperature from plain black. Clean the build plate with isopropyl alcohol between prints. Fingerprint oil is the usual reason a first layer refuses to stay down, and PETG shows it quickly.
🧵 Retraction and stringing
PETG is sticky when molten, so it leaves strings. Short retraction works best, around 1 to 2 mm on a direct drive and 4 to 6 mm on Bowden, at moderate speeds. Too much retraction pulls molten plastic back and causes clogs and blobs.
Lower the temperature a little before changing retraction. Combing mode in your slicer keeps travel moves inside the part and cuts strings across gaps.
A quick way to judge your settings is a stringing test with two thin towers about 30 mm apart. Print it, look at the threads between the towers, and change one value per run. Changing temperature, retraction and speed together hides which one helped. Also enable a small z-hop only if the nozzle drags over printed walls, because z-hop itself can leave tiny blobs on PETG.
🌬️ Cooling and layer strength
Cooling is a trade-off. Heavy fan makes PETG crisp but weak between layers, and it can crack. Use 30 to 50 percent, with the fan off for the first few layers. Bridges and small overhangs can take a little more.
Bridges are where PETG shows its character. It sags more than PLA, so give long bridges a higher fan speed for those moves only, and slow them down. Printing in a draught-free room helps. On a cold winter morning on the Highveld, an open window can split a tall PETG part, so close it or cover the machine.
💧 Dry filament and bed release
PETG absorbs moisture, and on the Durban coast an open spool can pick up enough humidity in a week to pop and string. Dry it for several hours at around 60 degrees, then store it in a sealed box with silica gel.
A simple test shows whether the spool is the problem. Extrude a few centimetres into the air and watch the strand. Clear, smooth filament means it is dry, while crackling, tiny bubbles or a hazy, rough strand means it is not. Do this at the start of each session in humid weather, since the answer changes with the season, and a dry spool saves you from chasing temperature fixes that cannot work. On a smooth PEI sheet, a thin layer of glue stick acts as a release layer so the part does not tear the surface. Compare machines among our 3D printers if your current one tops out below 250 degrees, and browse 3D printing filament for your first PETG spool.
Frequently Asked Questions
What temperatures suit PETG?
About 230 to 250 degrees nozzle, 70 to 85 bed. Confirm on the spool.
How much fan?
Around 30 to 50 percent, off for early layers.
How do I stop strings?
Dry the filament, trim temperature slightly and shorten retraction.
Why does it stick so hard?
A smooth PEI sheet bonds strongly. Use glue stick as a release and raise the first layer slightly.
Should I print slower than PLA?
A little, particularly on outer walls and the first layer.
Do I need an enclosure?
Not usually, only a room without draughts.
Ready to print tougher parts in PETG?
Visit Evetech's filament and 3D printer categories, pick a spool and make sure your machine reaches the nozzle temperature you need.