Most flexible filament prints best at a TPU print temp of roughly 210 to 230 degrees at the nozzle, but the number on your spool label outranks any general guide. Print a temperature tower once, pick the cleanest floor, and your next flexible spool will start from a known value.
Quick Answer
Start at 220 degrees, bed at 40 to 60 degrees, and print slowly, often 15 to 30 mm/s. Move in 5 degree steps using a temperature tower, since brands differ. If the surface shows bubbles or pops, the filament is damp and no temperature will cure it. A first spool of TPU typically sits in the R300 to R500 range.
🌡️ Finding your nozzle temperature
TPU is soft, so it melts quickly and strings readily. Too cool and the layers bond weakly and the part tears along the layer lines. Too hot and it oozes and leaves hairs across gaps.
A temperature tower is the honest test. Print a small stack where each block is printed 5 degrees hotter than the last, from about 200 to 240. Pull the print apart by hand. The best block is the lowest one where layers resist peeling and stringing is minimal. Write that number on the spool.
Hardness changes the answer a little. The common Shore 95A grade behaves like firm rubber and prints near the middle of the range, while softer grades such as 85A want slower speeds and often a slightly cooler nozzle. If the label gives a window, say 210 to 230, start at the midpoint instead of the top, because heat that is too high wastes the main benefit of TPU, a clean and springy layer bond.
🛏️ Bed temperature and surface
TPU grips most surfaces better than PLA does. A warm bed at 40 to 60 degrees is plenty, and a clean PEI sheet or glass plate holds the first layer without glue. Too much heat softens the lowest layers and gives an elephant-foot flare.
Print the first layer a touch slower than the rest. If the part is stubborn to remove, let the bed cool fully, because flexible prints release easily once cold.
Squish matters here. Set the nozzle height so the first layer is pressed down gently but not crushed, since TPU squeezed too hard spreads sideways and can jam the extruder gear later. A 0.2 mm first layer with slightly wider lines usually grips well on a cold morning in a Pretoria garage too, as long as the bed has reached its set temperature.
💧 Drying matters more than a few degrees
Wet TPU is the cause of most bad flexible prints. Moisture turns to steam inside the nozzle, which gives a crackling sound, tiny bubbles and a fuzzy surface. On the Durban coast, an opened spool left on a shelf in summer can be wet within days.
Dry it before you tune anything. A filament dryer at about 50 degrees for several hours works, and a household oven set to its lowest setting can do the same job if you watch it. Store the spool in a sealed box with silica gel after printing.
🐢 Speed, retraction and feed path
Flexible filament compresses in the feed path, so slow printing is the secret. Keep speeds low, often 15 to 30 mm/s, and cut retraction to a millimetre or two, or switch it off if stringing allows. A direct drive extruder handles this far better than a Bowden tube, though Bowden machines can manage with a short tube and a tight filament guide.
Check the filament path by hand before a long job. Feed the strand through the extruder with the nozzle cold and make sure it moves without a kink or a gap where it could buckle. Tighten the extruder tension just enough to grip, because a spring set too hard flattens the strand and causes under-extrusion that looks like a temperature problem but is not. Cooling should be low to medium. A fan at 30 to 50 percent keeps overhangs clean without weakening the bond between layers. Browse our 3D printing filament range for flexible spools, or compare 3D printers with a direct drive extruder if flexibles are your main goal.
Frequently Asked Questions
Where should I set TPU at first?
Around 220 degrees, or the middle of the spool label's range. Adjust with a temperature tower.
Does hotter make TPU stronger?
Only up to a point. Past that it strings and oozes, so choose the lowest temperature that still bonds well.
Why is my TPU popping?
Moisture. Dry the spool before you change any setting.
Does bed temperature matter?
Slightly. 40 to 60 degrees and a clean PEI sheet or glass plate is plenty.
Can a Bowden machine print TPU?
Sometimes, with very slow speeds, a short tube and a tight path. Direct drive is easier.
Do I use the part cooling fan?
Low to medium is usual. Test with a small piece and watch the overhangs.
Ready to print something that bends without breaking?
See the filament and 3D printer categories at Evetech, pick a flexible spool and a machine with a direct drive extruder, and run your first tower.