Strings, blobs, a hazy finish and layers that snap apart all share a short list of causes, so a calm, one-change-at-a-time method will fix petg printing issues faster than swapping profiles at random. Dry the spool first, then work through temperature, retraction and cooling in that order.
Quick Answer
Dry the filament for several hours, print a small test cube, and change only one setting per run. Typical fixes are a nozzle five degrees cooler for strings, slightly more heat for weak layers, and a lower fan speed. A spool of PETG sits around R300 to R500 locally, so a clean test routine saves real money.
💧 Start With the Spool, Not the Slicer
Water is behind more PETG faults than any slicer value. Wet filament crackles, throws tiny bubbles, leaves a rough or cloudy surface and strings like cheese. If a fresh spool prints cleanly and an old one does not, you have your answer.
South Africa's coast makes this worse. In Durban, an open spool left beside the printer for several days takes up enough moisture to cause pops, whereas dry Highveld air is kinder. Whatever your area, dry the spool in a filament dryer or a gentle oven, then keep it in an airtight box with desiccant. When you restock, a look through 3D printing filament is worth it for spools with tight diameter tolerance.
🧵 Stringing and Blobs
PETG oozes easily, so strings are the common complaint.
- Lower the nozzle temperature in steps of five degrees until strings thin out but layers still fuse.
- Raise retraction slowly. On a Bowden tube, a few millimetres more distance often helps, while direct drive needs far less.
- Increase travel speed so the nozzle spends less time hovering between parts.
Blobs and zits at the seam come from pressure building up and releasing. Try coasting if your slicer has it, slow the outer wall a little, and choose a seam position that falls in a hidden corner. Do not change more than one thing between prints.
🧱 Weak Layers and Poor Surface
If a part snaps cleanly along the layer lines, the plastic did not fuse. Heat is the lever: print five degrees hotter, slow the speed slightly and cut the cooling fan so each layer stays warm long enough to bond. Check for under-extrusion as well, because tiny gaps inside the wall weaken it as much as low heat.
A hazy or streaky outer wall can mean moisture, but also a dirty nozzle. Heat the nozzle, pull a cold-pull or clean it with a needle, and inspect the tip for burnt plastic. If a flow-rate test shows the printer is putting out too little or too much, trim the flow by a couple of percent until walls look smooth and consistent.
🌬️ Enclosures, Draughts and Over-Adhesion
PETG does not need a sealed enclosure, but it hates a cold draught across the part. A simple cardboard shield or a quiet corner of the room is enough. Avoid a closed box that overheats, since PETG prefers moderate temperatures around the print.
Over-adhesion is another PETG trait. Parts can weld themselves to smooth plates, so use a thin glue-stick layer as a release agent and let the bed cool before removal. If you suspect the printer itself is struggling, browsing 3D printers and parts can help you spot a worn nozzle or fan worth replacing.
Keep a short log of each test print, noting the temperature, retraction and fan value you changed. After three or four runs the pattern is clear, and you can save the result as a profile for that spool. A small calibration cube printed beside the real part also gives you a quick check of dimensions without wasting a full print on a fault you could have caught early.
Frequently Asked Questions
Why does PETG string more than PLA?
It is stickier and flows more readily when hot. A dry spool, a nozzle a few degrees cooler and tuned retraction usually remove most of the hairs.
What causes blobs and zits on PETG?
Pressure builds in the nozzle and then releases at the seam. Coasting, a slower outer wall and a hidden seam position reduce the marks.
How do I fix weak layer bonding?
Print slightly hotter and ease off the part fan so each layer fuses to the one below. Also rule out under-extrusion, which leaves gaps.
Why is my PETG hazy or rough?
Moisture scatters light and roughens the surface, so dry the spool. A dirty nozzle with burnt residue also leaves streaks.
Is humidity really a problem for PETG here?
Yes, especially along the coast. In Durban, spools left out for days absorb water and pop, so seal them with desiccant.
Should I use an enclosure for PETG?
It is not required. A draught-free spot is enough, and a fully sealed box can overheat the print.
Ready to troubleshoot PETG with confidence?
Check the 3D printing filament and 3D printer sections at Evetech for dependable spools and replacement parts.